Mahavir Metals India is a leading trader, distributor, and manufacturer of Stainless Steel Buttweld Pipe Fittings that provide faster machining speeds, longer tool life, better component quality, and reduced total cost of machined parts. Although Stainless Steel Elbow Buttweld Pipe Fittings is best known for its heat and oxidation resistance, it also has outstanding resistance to chloride stress – corrosion cracking, carburization, and reducing or carburizing atmospheres. Stainless Steel Tee Buttweld Pipe Fittings can be a cost-effective option for high-strength carbon steels and other stainless grades due to their strength, corrosion resistance, and ease of construction. Compared to ordinary grades, adding molybdenum and nitrogen in Stainless Steel Cross Buttweld Pipe Fittings means that more powerful processing equipment may be required. We also provide stainless steel buttweld pipe fittings, stainless steel 316 buttweld pipe fittings, stainless steel 310 buttweld pipe fittings, stainless steel 317 buttweld pipe fittings, and stainless steel 316TI buttweld pipe fittings. Buttweld Pipe Fittings, Stainless Steel 347 Buttweld Pipe Fittings, Stainless Steel 410 Buttweld Pipe Fittings, Stainless Steel 446 Buttweld Pipe Fittings, Stainless Steel 904L Buttweld Pipe Fittings, and other stainless steel pipe fittings. Reducer Buttweld Pipe Fittings in Stainless Steel is a low carbon, non-hardening stainless steel variant that remains flexible and ductile even when rapidly cooled.
Specifications | : | ASTM A403 / ASME SA403 |
Size | : | 1/8” NB TO 48” NB. (Seamless & 100% X-Ray Welded, Fabricated) |
Standards | : | ASME/ANSI B16.9, ASME B16.28, MSS-SP-43 |
Thickness | : | 5s, 10s, 40s, 80s, 10, 20, 40, STD, 60, 80, XS, 100, 120, 140, 160, XXS available with NACE MR 01-75 |
Type | : | Seamless / Welded / Fabricated |
Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N |
SS 304 | 0.08 max | 2 max | 0.75 max | 0.045 max | 0.030 max | 18 – 20 | – | 8 – 11 | – |
SS 304L | 0.035 max | 2.0 max | 1.0 max | 0.045 max | 0.03 max | 18 – 20 | – | 8 – 13 | – |
SS 304H | 0.10 max | 2.0 max | 0.75 max | 0.045 max | 0.03 max | 18 – 20 | – | 8 – 10.5 | – |
SS 310 | 0.015 max | 2.0 max | 0.15 max | 0.020 max | 0.015 max | 24.00 – 26.00 | 0.10 max | 19.00 – 21.00 | 54.7 min |
SS 310S | 0.08 max | 2.0 max | 1.00 max | 0.045 max | 0.030 max | 24.00 – 26.00 | 0.75 max | 19.00 – 21.00 | 53.095 min |
SS 310H | 0.04 – 0.10 | 2.0 max | 1.00 max | 0.045 max | 0.030 max | 24.00 – 26.00 | – | 19.00 – 21.00 | 53.885 min |
SS 316 | 0.08 max | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 16.00 – 18.00 | 2.00 – 3.00 | 11.00 – 14.00 | 67.845 min |
SS 316L | 0.035 max | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 16.00 – 18.00 | 2.00 – 3.00 | 10.00 – 14.00 | 68.89 min |
SS 316H | 0.10 max | 2.0 max | 0.75 max | 0.045 max | 0.030 max | 16.00 – 18.00 | 2.00 – 3.00 | 10.00 – 14.00 | 68.89 min |
SS 316Ti | 0.08 max | 2.0 max | 0.75 max | 0.045 max | 0.030 max | 16.00 – 18.00 | 2.00 – 3.00 | 10.00 – 14.00 | 68.395 min |
SS 317 | 0.08 max | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 18.00 – 20.00 | 3.00 – 4.00 | 11.00 – 15.00 | 57.845 min |
SS 317L | 0.035 max | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 18.00 – 20.00 | 3.00 – 4.00 | 11.00 – 15.00 | 57.89 min |
SS 321 | 0.08 max | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 17.00 – 19.00 | 0.10 max | 9.00 – 12.00 | 5(C+N) – 0.70 max |
SS 321H | 0.04 – 0.10 | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 17.00 – 19.00 | 0.10 max | 9.00 – 12.00 | 4(C+N) – 0.70 max |
SS 347 | 0.08 max | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 17.00 – 20.00 | 10xC – 1.10 | 9.00 – 13.00 | 62.74 min |
SS 347H | 0.04 – 0.10 | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 17.00 – 19.00 | 8xC – 1.10 | 9.0 -13.0 | 63.72 min |
SS 904L | 0.020 max | 2.00 max | 1.00 max | 0.040 max | 0.030 max | 19.00 – 23.00 | 4.00 – 5.00 max | 23.00 – 28.00 | 1.00 – 2.00 |
Grade | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
SS 304 | 8.0 g/cm3 | 1400 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35% |
SS 304L | 8.0 g/cm3 | 1400 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35% |
SS 304H | 8.0 g/cm3 | 1400 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 40% |
SS 310 | 7.9 g/cm3 | 1402 °C (2555 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 40% |
SS 316 | 8.0 g/cm3 | 1400 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35% |
SS 316L | 8.0 g/cm3 | 1399 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35% |
SS 316H | 8.0 g/cm3 | 1400 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35% |
SS 316Ti | 8.0 g/cm3 | 1399 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35% |
SS 317 | 7.9 g/cm3 | 1400 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35% |
SS 321 | 8.0 g/cm3 | 1457 °C (2650 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35% |
SS 347 | 8.0 g/cm3 | 1454 °C (2650 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35% |
SS 904L | 7.95 g/cm3 | 1350 °C (2460 °F) | Psi – 71000 , MPa – 490 | Psi – 32000 , MPa – 220 | 35% |